If you’ve ever stood in a plastics recycling or manufacturing plant, watching bales of post-consumer plastic or trimmed industrial scrap get loaded into a granulator, you might have noticed one thing that trips up even the most experienced operators: moisture. I’m the owner of a plastics granulator supply business, and I can’t tell you how many times I’ve gotten a call from a customer who just destroyed a batch of resin, or fried a granulator’s blades, because they skipped checking moisture content before feeding material into their machine. It’s one of those “small detail, huge impact” parts of plastics processing that everyone talks about, but few actually nail down consistently. Today, I want to break down what the moisture content requirement actually is for plastics before they hit a granulator, why it matters, and what I’ve learned from working with hundreds of plants over the last 12 years to get this right. Plastic Granulator

First, let’s define what we’re even talking about when we say moisture content for plastics. It’s not like the moisture you’d see on a wet towel or a puddle—we measure it as a percentage of the plastic’s total weight, usually from 0.01% up to maybe 1% for some applications. For context, that’s roughly one drop of water per gallon of plastic, so it’s extremely low, but it’s enough to cause major problems if it’s too high. A lot of new operators think “if it looks dry, it’s dry,” but that’s a myth. Ambient humidity, even in a dry warehouse, can seep into plastic pellets, regrind, or bales of scrap over time, especially if the plastic is hygroscopic. Hygroscopic plastics are the big culprits here—think PET (polyethylene terephthalate), nylon (PA), polycarbonate (PC), and thermoplastic polyurethanes (TPU). These materials literally absorb water from the air, like a sponge, and they hold onto it tight. Non-hygroscopic plastics, like HDPE, PP, and PS, absorb almost no water at all, so their moisture content requirements are way less strict. That’s the first big mistake I see: treating all plastics the same when it comes to moisture.

Let’s start with why moisture matters before granulation, because a lot of people assume the problems start during melting (which is true for extrusion or injection molding), but granulation has its own set of issues, even when you’re just chopping plastic into small flakes or pellets. First, there’s the risk of machine damage. When wet plastic hits the rotating blades and the cutting chamber of a granulator, any trapped moisture flashes into steam almost instantly, thanks to the heat generated by friction from the blades spinning at high speeds. That steam creates tiny pressure spikes inside the granulator chamber. If it’s bad enough, those spikes can warp the cutting chamber, crack the blade holders, or even cause the blades to chip. I had a customer two years back who was granulating wet PET bottle bales that had been stored in an outdoor yard for three weeks, and the steam pressure from the moisture blew a small hole in the side of their granulator’s cutting chamber. They had to shut down production for three days waiting for a replacement part, and that cost them more than the scrap plastic was worth. That’s avoidable if you check moisture before you feed it in.

Next, there’s the problem of contamination in the regrind. When water flashes to steam during granulation, it carries tiny bits of plastic dust and residue with it, which get trapped in the regrind flakes. That residue makes the regrind less pure, which is a big deal if you’re selling it back to a manufacturer who needs consistent material. I’ve had customers come to me with regrind that was supposed to be 99.5% pure, but tested at 98.8% because of moisture-related contamination, and they couldn’t sell it for full price. The other side of that is degradation of the plastic itself. For hygroscopic plastics like nylon, the moisture that’s absorbed into the polymer chain breaks the molecular bonds when heated, even during the short time it takes to granulate. That makes the regrind weaker, less flexible, and more prone to breaking in downstream uses like 3D printing or film production. For non-hygroscopic plastics, this degradation is almost non-existent, but the other issues still apply.

Now, let’s get to the actual numbers. This is where a lot of guides get vague, so I’ll share what I’ve learned from field testing and working with process engineers across the industry. For non-hygroscopic plastics (HDPE, PP, PS, HIPS), the general maximum moisture content before granulation is 0.2% by weight. These plastics barely absorb water, so if you store them properly in airtight containers, they’ll usually come in at 0.05% to 0.1%, which is perfect. The only time you need to worry about their moisture content is if they’ve been submerged, like post-consumer plastic from a water bottle recycling line that got rained on before baling. For these, you just need to let them air dry for a few hours, or use a small centrifugal dryer to pull off surface moisture, and they’ll be fine.

For hygroscopic plastics, that number is way lower, and it depends on the type of plastic and what you’re going to do with the regrind after granulation. PET is the most common one here. The maximum moisture content for PET before granulation is 0.05% by weight. I know that sounds tiny, but it’s non-negotiable. If PET has more than 0.05% moisture, the steam during granulation not only causes pressure spikes, but when you melt the regrind later (say, for making new water bottles), you get splay marks—those little white streaks on the surface of the plastic that make it unmarketable. That’s a $100,000+ loss for a plant that makes 10 million water bottles a month, because all the defective product has to be scrapped. For nylon and polycarbonate, the number is even stricter: 0.02% to 0.03% by weight. These materials absorb moisture so quickly that even if you store them for a day in a warehouse with 60% humidity, they can jump to 0.08% moisture, which is too high for granulation. I always tell customers working with nylon to keep their scrap in airtight gaylords, not just stacked on the floor, and to test moisture content within 24 hours of when they plan to granulate.

Wait, but what if you’re granulating mixed plastic scrap? A lot of recycling plants process mixed post-consumer material that has a mix of hygroscopic and non-hygroscopic plastics. That’s a trickier case, because you can’t have a one-size-fits-all number. In that scenario, I usually recommend targeting the lowest common denominator: 0.05% moisture max. Because even if most of the scrap is HDPE, any PET or nylon in the mix will cause issues if it’s over that threshold. Alternatively, some plants will dry the mixed scrap in a continuous air dryer before granulation, which pulls moisture down to the required level. It’s an extra step, but it’s way cheaper than replacing a granulator or losing money on defective regrind.

Now, the question is: how do you actually test moisture content before granulation? A lot of operators use the “touch test”—squeezing a handful of plastic and feeling if it’s damp—but that’s not accurate enough. For critical applications (hygroscopic plastics), you need a lab-grade moisture analyzer, which costs between $1,500 and $5,000, and it gives you a reading in 5 to 10 minutes. For less critical non-hygroscopic plastics, a moisture meter (like a grain moisture meter, adapted for plastics) will work, which is cheaper, around $200, and gives a reading in 30 seconds. I always advise customers to invest in a moisture analyzer if they work with PET, nylon, or PC—paying for that tool once saves them from thousands in repair costs and lost production.

I also want to address a common myth: some people think that drying the plastic after granulation is just as good as drying it before. That’s not true. Once plastic is granulated, it has a much higher surface area than solid pellets or scrap, so it absorbs moisture even faster. If you feed wet plastic into a granulator, the moisture is already trapped inside the polymer chains, and the steam from friction causes degradation that drying after can’t fix. Drying after is a good step for downstream processing, but it doesn’t solve the granulation-related problems or the initial degradation. I’ve seen customers try this, and they end up with regrind that’s weaker and has more contamination than if they’d just checked moisture before feeding it.

Over the years, I’ve worked with a lot of customers who tried to cut corners on moisture testing, and every time, it comes back to bite them. One customer in Ohio was granulating post-consumer PET with a moisture content of 0.12% because they skipped testing, and within six months, their granulator’s cutting blades had worn out 30% faster than expected, and they had to replace the cutting chamber. When they did the math, the cost of new blades and the lost production from downtime was 15 times the cost of a moisture analyzer. That’s not a good investment. On the flip side, a customer in Texas that started testing moisture and implementing drying steps before granulation saw a 20% drop in blade replacement costs, and their regrind was selling for 5% more because of its higher purity.

So, to wrap this up, the moisture content requirement for plastics before entering a granulator isn’t a random number—it’s tailored to the type of plastic you’re processing. Non-hygroscopic plastics (HDPE, PP, PS) need a maximum of 0.2% moisture by weight. Hygroscopic plastics (PET, nylon, PC) need a maximum of 0.02% to 0.05%, depending on the material. For mixed scrap, target 0.05% to cover all bases. The key is to stop relying on visual or tactile checks, invest in a simple moisture testing tool, and plan to dry the plastic if it’s over the required level.

If you’re a plant manager or operator dealing with granulation issues, or you’re looking to upgrade your granulator with features that handle moist material better (like reinforced cutting chambers or integrated moisture vents), I’m here to help. I’ve spent years designing granulators for all types of plastics, and I work directly with customers to set up processes that eliminate moisture-related problems. Reach out to my team to discuss your specific needs, and we can help you find the right solution for your operation.

Blower References

  1. Plastics Industry Association. (2021). "Moisture Management in Plastics Processing and Recycling." Plastics Processing Guide Series.
  2. Rosato, D. V., & Rosato, M. G. (2019). Plastics Materials and Processes: A Concise Encyclopedia, 3rd Edition. William Andrew Publishing.
  3. American Society for Testing and Materials (ASTM). (2020). Standard Test Method for Moisture Content of Plastics by Thermogravimetry (ASTM D6980-20).
  4. The Recycling Partnership. (2022). "Best Practices for Moisture Control in Post-Consumer Plastic Recycling Facilities." Recycling Operations Report.

Wenzhou Shimeina Machinery Automation Technology Co., Ltd.
As one of the most experienced plastic granulator manufacturers and suppliers in China, we warmly welcome you to buy durable plastic granulator for sale here from our factory. All machines are with high quality and low price.
Address: No.56, Xingsheng Road, Centou Village, Tangxia Town, Ruian City, Wenzhou, Zhejiang Province
E-mail: info@shimeina.com
WebSite: https://www.shimeina.com/